An optimised thin film wavelength shifting coating for Cherenkov detection

Manuel Grande*, Gary R. Moss

*Awdur cyfatebol y gwaith hwn

Allbwn ymchwil: Cyfraniad at gyfnodolynErthygladolygiad gan gymheiriaid

15 Dyfyniadau (Scopus)

Crynodeb

Investigations of an appropriate thin film wavelength shifting (WLS) coatings for Cherenkov radiation detection are reported. A number of dyes were investigated and an optimum coating arrived at. This consists of 0.175 mg/cm2 of p-terphenyl, 0.095 mg/cm2 of bis-MSB and 16 mg of acrylic matrix (Paraloid B 72) for coating on a perspex substrate. Coating over Pilot 425 is best done with a bis-MSB grammage reduced to 0.052 mg/cm2. These coatings gave an average quantum efficiency of 91% of that a quartz window PM tube over a wavelength interval of 200-400 nm. A number of hints on the techniques of utilising thin film WLS coatings are also included.

Iaith wreiddiolSaesneg
Tudalennau (o-i)539-548
Nifer y tudalennau10
CyfnodolynNuclear Instruments and Methods In Physics Research
Cyfrol215
Rhif cyhoeddi3
Dynodwyr Gwrthrych Digidol (DOIs)
StatwsCyhoeddwyd - 01 Hyd 1983